涂层钢
货号 | 直径 | 不。 | of | 行 | 面宽 | 金属丝 | 厚度 |
mm | mm | mm |
带多心轴环 13, 16
661000 | 75 | 5 | 16 | 0.30 |
661003 | 100 | 5 | 16 | 0.30 |
661006 | 125 | 5 | 19 | 0.30 |
带多心轴环 13, 16, 19, 22, 25, 32, 50
661009 | 150 | 5 | 20 | 0.30 |
661012 | 175 | 5 | 20 | 0.30 |
661015 | 200 | 5 | 20 | 0.30 |
661018 | 250 | 5 | 25 | 0.30 |
661021 | 300 | 5 | 25 | 0.30 |
不锈钢
货号 | 直径 | 不。 | of | 行 | 面宽 | 金属丝 | 厚度 |
mm | mm | mm |
带多心轴环 13, 16
661024 | 75 | 5 | 16 | 0.30 |
661027 | 100 | 5 | 16 | 0.30 |
661030 | 125 | 5 | 19 | 0.30 |
带多心轴环 13, 16, 19, 22, 25, 32, 50
661033 | 150 | 5 | 20 | 0.30 |
661036 | 175 | 5 | 20 | 0.30 |
661039 | 200 | 5 | 20 | 0.30 |
661042 | 250 | 5 | 25 | 0.30 |
661045 | 300 | 5 | 25 | 0.30 |
黄铜涂层
货号 | 直径 | 不。 | of | 行 | 面宽 | 金属丝 | 厚度 |
mm | mm | mm |
带多心轴环 13, 16
661048 | 75 | 5 | 16 | 0.30 |
661051 | 100 | 5 | 16 | 0.30 |
661054 | 125 | 5 | 19 | 0.30 |
带多心轴环 13, 16, 19, 22, 25, 32, 50
661057 | 150 | 5 | 20 | 0.30 |
661060 | 175 | 5 | 20 | 0.30 |
661063 | 200 | 5 | 20 | 0.30 |
661066 | 250 | 5 | 25 | 0.30 |
661069 | 300 | 5 | 25 | 0.30 |
锯片的使用与保养
◎ 锯片的硬质合金尖端非常锋利,使用过程中必须防止硬质合金尖端。
◎ 定期清扫和支撑机器,主轴运行公差必须小于h7。
◎ 法兰必须相互平行,直径必须相同,为锯片直径的1/3(公式——纵切锯片为1/2.
◎ 安装锯片时,应高于板面5-6齿。
◎ 操作前检查锯片是否牢固,确保机器前无人。运行时不要进给检查机器是否适合运行。定期检查机器功能,跳动小于±0.02MM,襟翼小于±0.01。
◎ 连续使用后,必须将锯片拆下清洗,清除锯片两侧的树脂和锯屑,否则会影响锯片的使用效果。
◎ 锯片的存放,不能分层锯片,放在原包装里面。
锯片的翻新
◎ 硬质合金锯片的翻新 不再磨锐,横片变粗。使用锯片机的功率明显增加。加工物料时,物料出现爆裂。硬质合金尖端排气超过0.02MM。
◎ 翻新锯片应由正规公司修磨,确保翻新后的锯片质量。